RFA, XRF, Röntgenfluoreszensanalyse RFA Ringversuch St. Gobain - SGIB, Borosilikatglas
Veranstalter des Ringversuchs:
St. Gobain Isover - CRIR
Ringversuchsmaterial:
SGIB, Borosilikatglas
RV geschlossen:
2002 - 6
Literatur:
Abschlussbericht
Hauptelemente [MA%]
| CRB | RV | 1sRV | Z-Score | |
| Na₂O | 15,780 | 15,810 | 0,130 | --- |
| MgO | 3,080 | 3,200 | 0,100 | --- |
| Al₂O₃ | 1,610 | 1,600 | 0,070 | --- |
| SiO₂ | 65,440 | 65,780 | 0,320 | --- |
| P₂O5 | 0,030 | 0,030 | 0,007 | --- |
| SO₃ | 0,090 | 0,080 | 0,030 | --- |
| K₂O | 0,600 | 0,610 | 0,030 | --- |
| CaO | 7,660 | 7,600 | 0,150 | --- |
| TiO₂ | 0,028 | 0,030 | 0,007 | --- |
| Fe₂O₃ tot. | 0,210 | 0,240 | 0,020 | --- |
| MnO | 0,407 | 0,410 | 0,023 | --- |
Spurenelemente [µg/g]
| CRB | RV | 1sRV | Z-Score | |
| Ba | 200,00 | --- | --- | --- |
| Cr | 90,00 | --- | --- | --- |
| Rb | 10,00 | --- | --- | --- |
| Sr | 10,00 | --- | --- | --- |
| Zr | 320,00 | --- | --- | --- |
Legende
CRB
Ergebnisse CRB
Ringversuch
Ergebnisse Ringversuch
1s-RV
Standardabweichung Ringversuch
Z-Score
Differenz des Messwerts vom Mittelwert des Ringversuchs
*
Wert nicht zertifiziert